Reproduce the work
These small examples teach methods from my research. Each tutorial lists the files, commands, and expected output. The status tells you which example was run.
Before you start: the ML-potential tutorials use the open MACE-MP-0 model by default (no account needed). Pass --model uma-s-1p1 to use Meta’s UMA, the model in several of the papers. UMA requires a free Hugging Face token. LAMMPS tutorials need a LAMMPS build; see LAMMPS_SETUP.md.
Benchmark a universal ML potential on doped MoS₂
Build doped MoS₂ cells, relax them with an ML potential, compute dopant formation energies, then heat a doped bilayer and watch the dopants move.
Stretch MoS₂ until it breaks, at three temperatures
Pull a monolayer MoS₂ sheet apart at 100, 200 and 300 K with an ML potential, and measure flake tilt with a PCA method.
How force fields and mixing rules change gold–ion interactions
Recompute the Au–ion Lennard-Jones cross terms for the four ion force fields in the paper’s Table I, and see how far they disagree.
Diagnose a foundation potential on a molten salt
Melt LiCl–FeCl₂ with an off-the-shelf ML potential and compute the partial radial distribution functions that reveal whether Fe ions cluster.
From g(r) to thermodynamics: Kirkwood–Buff integrals
Simulate the LiCl–KCl eutectic melt and compute running Kirkwood–Buff integrals, the bridge from structure to activity coefficients and phase diagrams.
Let the model choose its next training data
Run Pt(111)–water MD, measure where two ML potentials disagree, and select the most uncertain frames for DFT labeling.
Check, then fine-tune, a foundation potential
Compare model predictions with reference labels in a parity plot (the demo compares two foundation models), then follow the LoRA fine-tuning recipe used for MoS₂ with N₂.
Grow a Ni-doped MoS₂ film atom by atom
Deposit Mo, S and Ni atoms onto a MoS₂ substrate one at a time, then measure Ni clustering and MoS₂-like order.
Build a temperature plot matrix from literature data
Turn digitized friction, wear-rate and wear-life data into the review’s metric × environment plot matrix.
Pull an Inconel-718 nanowire at 100 K and 800 K
Build a random Ni–Cr–Fe alloy nanowire, stretch it at two temperatures with the Bonny FeNiCr EAM potential, and compare the stress–strain curves.
Quench liquid tin at two rates, then stretch it
Melt Sn, cool it at 10 and 100 K/ps with a MEAM potential, and compare strength and stiffness of the two solids.
Stretch CdTe and CdSe₀.₅Te₀.₅ nanowires
Compare the tensile strength of a zinc-blende CdTe nanowire before and after random Se substitution, with the Cd–Te–Se bond-order potential.
Deposit an alloy layer by layer, then test it
Mimic additive manufacturing: deposit Ni–Cr–Fe atoms in batches, cool at two rates, and run a tensile test.
Cycle a gold–silver core–shell nanowire (draft)
Tension–compression cycling of Au-core/Ag-shell and Ag-core/Au-shell nanowires with the paper’s MEAM parameters. Draft: some alloy parameters still need checking against the published tables.