The problem
Solder joints experience repeated mechanical and thermal loads. Cooling history changes the structure that carries those loads.
What I did
LAMMPS molecular dynamics heated and cooled pure tin, tin–silver, and SAC305 models. A modified embedded atom method potential was used for tensile and cyclic loading after cooling.
The drop as cooling increased from 2.5 to 100 K/ps shows that the rapidly cooled tin model carried less tensile stress before failure.
SAC305 weakened as cooling increased from 2.5 to 100 K/ps, while retaining the highest tensile strength of the three simulated materials.
The decrease as cooling increased from 2.5 to 100 K/ps shows that the simulated SAC305 became less stiff.
What we found
- When cooling increased from 2.5 to 100 K/ps, pure tin tensile strength fell from 6.42 to 5.60 GPa.
- Over the same cooling-rate change, SAC305 tensile strength fell from 6.91 to 6.16 GPa and remained highest among the three materials.
- SAC305 Young's modulus fell from 108.96 to 97.65 GPa over that cooling-rate range.
- Toughness increased by 14.03% for tin, 12.87% for tin–silver, and 8.75% for SAC305.
Why it matters
The trends inform studies of how solidification conditions affect solder-joint reliability.
Recreate it yourself. Melt Sn, cool it at 10 and 100 K/ps with a MEAM potential, and compare strength and stiffness of the two solids. Open the tutorial →
Next case study · Selenium makes CdTe nanowires stronger and stiffer → · Back to Nanoscale mechanics research