PublishedComputational Materials Science · 244, 113229 · 2024

Intermediate nickel lowers shear stress in sputtered MoS₂

Nickel changed the structure and sliding response of simulated sputtered MoS₂ films. Intermediate nickel contents formed a particle associated with lower shear stress.

Tutorial Journal article

The problem

Nickel can change the structure of sputtered MoS₂ lubricant films. The relationship between nickel content and sliding resistance matters when designing coatings.

What I did

Reactive molecular dynamics simulated deposition at different nickel contents and temperatures. The authors then compressed and sheared the films to examine their structure and sliding response.

2% and 10% by weightNickel contents associated with lower shear stress

The intermediate nickel contents outperformed the undoped and 15% films in this simulated shear comparison.

What we found

  1. Films with 2% and 10% nickel by weight had lower simulated shear stress than films with 0% and 15% nickel.
  2. The lower-stress films formed a particle during shear.
  3. The particle had a crystalline core and an amorphous nickel-containing surface.
  4. The authors associated particle formation with the combination of density, crystallinity, and nickel clustering in the intermediate-content films.

Why it matters

The results help select nickel contents for experimental testing of dry-film lubricant coatings.

Recreate it yourself. Deposit Mo, S and Ni atoms onto a MoS₂ substrate one at a time, then measure Ni clustering and MoS₂-like order. Open the tutorial →