The problem
Printed Inconel-718 cools after each layer is deposited. The study asked how the cooling rate changes the metal’s structure and tensile properties.
What I did
The simulations used an embedded-atom method (EAM) potential in LAMMPS. Layers were deposited on a pristine substrate, equilibrated at 2000 K, and cooled to 300 K. The cooling schedules spanned 5–100 K/ps and included a variable rate. A 22 × 5.5 × 5.5 nm bar was cut from the solidified layer and pulled along [001] at strain rates from 10⁸ to 10¹⁰ s⁻¹.
What we found
- Printed Inconel-718 had lower yield strength and elongation than conventional material. Its ultimate tensile strength was comparable.
- Faster cooling produced lower density, more defects, and a lower Young’s modulus.
- Slower cooling produced properties close to those of the pristine material.
- Sliding on {111} planes caused necking before fracture.
Why it matters
The simulations link the cooling schedule to defects and stiffness in printed Inconel-718.
Recreate it yourself. Mimic additive manufacturing: deposit Ni–Cr–Fe atoms in batches, cool at two rates, and run a tensile test. Open the tutorial →